Abatron AboThane 8901-4 Polyurethane Enamel
Subcategory: Polyurethane, TP; Thermoplastic
Material Notes: Clear, glossy polyurethane enamel with superb chemical, weather and abrasion resistance unsurpassed as a clear anti-graffiti coating. High-grade, high-build, 2-component system for superior performance on metal, wood, plastics, concrete in normal, industrial, all-weather and corrosive environments. Remarkable combination of weather, UV and chemical resistance. Suggested Uses: Protective or decorative coating of decks, indoor and outdoor furniture, boats, sports and playground equipment, structural and decorative components, tanks, plant equipment, railroad equipment and boxcars, trucks, buses, motor homes, plastic domes, components and structures, appliances, construction and farm equipment, metal furniture, floors in factories, offices, hospitals, warehouses, service stations, restaurants, public and private buildings. Processing: Ratio by volume: 100/50 Part A (clear resin solution)/Part B (clear coreactant solution)Information provided by Abatron.
| Available Properties |
- Density
- Solids Content
- Volatile Organic Compounds (VOC) Content
- Viscosity
- Pot Life
- Koenig Pendulum Hardness
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|