Abatron AboCast A/B Filled Potting Compound
Subcategory: Adhesive; Thermoset
Material Notes: Standard colored seamless casting resin. 100/40 ratio. Information provided by Abatron.
| Available Properties |
- Filler Content
- Hardness, Shore D
- Maximum Service Temperature, Air
- Pot Life
- Color
- Viscosity
|
|
|
|