QSI Quantum Silicones QSil 12 Clear Low Viscosity for Potting Material
Subcategory: Silicone; Thermoset
Material Notes: Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, variable cure speed with mild heat, transparent, room temperature cure, no solvents, good adhesion with use of a primer.
| Available Properties |
- Specific Gravity
- Viscosity
- Hardness, Shore A
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Pot Life
- Color
|
|
|
|
| Property Data |