QSI Quantum Silicones QSil 216 Transparent Liquid Silicone Rubber
Subcategory: Silicone; Thermoset
Material Notes: Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, no solvents, non-yellowing catalyst system, provides hydraulic stability and reversion resistance.
| Available Properties |
- Specific Gravity
- Viscosity
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Yield
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Shrinkage
- Refractive Index
- Pot Life
- Color
|
|
|
|