QSI Quantum Silicones QLE 1020 45 Durometer Clear, Addition Cure Elastomer for Coating
Subcategory: Silicone; Thermoset
Material Notes: Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: long pot life, excellent adhesion, good abrasion resistance. Applications: fabric or cloth coating.
| Available Properties |
- Specific Gravity
- Viscosity
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Yield
- Tear Strength
- Pot Life
- Color
|
|
|
|