QSI Quantum Silicones QM 100 Clear 30 Durometer Condensation Cure Material
Subcategory: Silicone; Thermoset
Material Notes: Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, fast demold time. Applications: special effects, fake ice, fake glass, where pigment is required.
| Available Properties |
- Specific Gravity
- Viscosity
- Hardness, Shore A
- Dry Time
- Pot Life
- Color
- Linear Shrinkage, inches, max
|
|
|
|