EPI Engineered Polymers EP IS Integral Skin Flexible Foam
Subcategory: Thermoset
Material Notes: EP-IS is integral skin flexible foam, “Powered by Reactamine ® Technology”, designed to give excellent surface skin. EP-IS contains cyclopentane as its blowing agent, which conforms to EPA standards for no CFC or HCFC blowing agents. Density can be varied from 5 – 30 PCF to obtain different hardness in the finished product.Part of the Amber Chemical Group. Data provided by manufacturer.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Yield
- Tear Strength
- Mold Temperature
- Dry Time
- Cure Time
|
|
|
|