EPI Engineered Polymers EP MAP-8.5 Aliphatic Polymers
Subcategory: Thermoset
Material Notes: EP MAP, “Powered by Reactamine® Technology”, are modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. EP MAP-8.5 contains 8.5% NCO. Part of the Amber Chemical Group. Data provided by manufacturer.
| Available Properties |
- Specific Gravity
- Viscosity
- Melting Point
- Flash Point
- Color
|
|
|
|
| Property Data |