EPI Engineered Polymers EP MAP-Z 14 Aliphatic Polymers

 

Subcategory: Thermoset

Material Notes:
EP MAP Z, “Powered by Reactamine® Technology”, are zinc modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. Three products are available. EP MAP Z has been designed for use as a primer for steel to prevent corrosion. Colors may be added due to its aliphatic nature. A clear top-coat of EP RAP60M may be used over EP MAP Z. Solvents such as xylene, MEK, or butyl acetate may be used to cut EP MAP Z to improve sprayability. EP Map-Z 14 contains 14 % NCO

Part of the Amber Chemical Group. Data provided by manufacturer.

Available Properties
  • Specific Gravity
  • Viscosity
  • Melting Point
  • Flash Point
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。