MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

EPI Engineered Polymers EP EF SP Extra Flex with Silicone, SMP™

 

Subcategory: Silicone; Thermoset

Material Notes:
EP EF SP, “Powered by Reactamine® Technology”, is a two component 100% solid Silicone Polyurea with superior performance in industrial applications. EP EF SP displays extremely fast cure times with excellent adhesions to different substrates. EP EF SP can be spray applied at temperatures ranging from 20°F to 150°F. EP EF SP has better chemical and water resistance than conventional. EP EF SP has a temperature range of -60°F to 250°F. EP EF SP conforms to USDA and FDA guidelines for incidental food contact. Silicone Polyureas have better weatherability.

Applications: EP EF SP adheres well to several substrates including concrete, steel, and wood. Some typical uses include:

  • SECONDARY CONTAINMENT
  • WASTEWATER LAGOON AND POOL LININGS
  • TABLE EDGING
  • COLD STORAGE AREAS
  • WASH BAY AND SHOWER LININGS
  • COOLING TOWERS
  • PETROCHEMICAL REFINERIES
  • OILFIELD PIPELINE COATINGS
  • WATER PROOFING
  • SEWER LINERS
  • MANHOLE RESTORATION
  • INDUSTRIAL FLOORING
  • BRIDGE COATINGS

    Part of the Amber Chemical Group. Data provided by manufacturer.

    Available Properties
    • Viscosity
    • Hardness, Shore A
    • Tensile Strength, Yield
    • Elongation at Yield
    • 100% Modulus
    • 300% Modulus
    • Adhesive Bond Strength
    • Tear Strength
    • Taber Abrasion, mg/1000 Cycles
    • Flash Point
    • Cure Time
    • Gel Time
    • Color
    • Flexibility
    • Resistance to 1,1,1-Trichlorethane
    • Resistance to Acetic Acid (100%)
    • Resistance to Acetone
    • Resistance to Ammonium Hydroxide (50%)
    • Resistance to Benzene
    • Resistance to Brine-Saturated H2O
    • Resistance to Chlorinated H2O
    • Resistance to Clorox® (10%) H2O
    • Resistance to Diesel Fuel
    • Resistance to Gasoline
    • Resistance to Gasoline/ 5% Methanol
    • Resistance to Gasoline/5% MTBE
    • Resistance to H2O
    • Resistance to H2O (14 days at 82°C)
    • Resistance to Hydraulic Fluid (oil)
    • Resistance to Hydrochloric Acid (20%)
    • Resistance to Hydrofluoric Acid(10%)
    • Resistance to Isopropyl Alcohol
    • Resistance to Lactic Acid
    • Resistance to MEK
    • Resistance to Methanol
    • Resistance to Methylene Chloride
    • Resistance to Mineral Spirits
    • Resistance to Motor Oil
    • Resistance to MTEB
    • Resistance to Muriatic Acid (10%)
    • Resistance to NaCl/H2O (10%)
    • Resistance to Nitric Acid (20%)
    • Resistance to Phosphoric Acid (10%)
    • Resistance to Phosphoric Acid (50%)
    • Resistance to Potassium Hydroxide (10%)
    • Resistance to Potassium Hydroxide (20%)
    • Resistance to Propylene Carbonate
    • Resistance to Skydrol®
    • Resistance to Sodium Bicarbonate
    • Resistance to Sodium Hydroxide (25%)
    • Resistance to Sodium Hydroxide (50%)
    • Resistance to Sodium Hypochlorite (10%)
    • Resistance to Steric Acid
    • Resistance to Sugar/H2O
    • Resistance to Sulfuric Acid (>50%)
    • Resistance to Sulfuric Acid (10%)
    • Resistance to Toluene
    • Resistance to Trisodium Phosphate
    • Resistance to Vinegar/ H2O (5%)
    • Resistance to Xylene
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
  • 请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。