EPI Engineered Polymers EP EF Extra Flex Polyurea
Subcategory: Thermoset
Material Notes: EP EF, Extra Flex Polyurea, “Powered by Reactamine® Technology, is a two component 100% solid Polyurea, with superior performance in industrial applications. EP EF displays extremely fast cure times with excellent adhesions to different substrates. EP EF can be spray applied at temperatures ranging from 20°F to 150°F. EP EF has excellent chemical and water resistance. EP EF has a temperature range of -40°F to 350°F. EP EF conforms to USDA and FDA guidelines for incidental food contact. Applications: EP EF adheres well to several substrates including concrete, steel, and wood. Some typical uses include: SECONDARY CONTAINMENT WASTEWATER LAGOON AND POOL LININGS TABLE EDGING COLD STORAGE AREAS WASH BAY AND SHOWER LININGS COOLING TOWERS PETROCHEMICAL REFINERIES OILFIELD PIPELINE COATINGS WATER PROOFING SEWER LINERS MANHOLE RESTORATION INDUSTRIAL FLOORING BRIDGE COATINGSPart of the Amber Chemical Group. Data provided by manufacturer.
| Available Properties |
- Viscosity
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Yield
- 100% Modulus
- 300% Modulus
- Adhesive Bond Strength
- Tear Strength
- Taber Abrasion, mg/1000 Cycles
- Flash Point
- Cure Time
- Gel Time
- Color
- Flexibility
- Resistance to 1,1,1-Trichlorethane
- Resistance to Acetic Acid (100%)
- Resistance to Acetone
- Resistance to Ammonium Hydroxide (50%)
- Resistance to Benzene
- Resistance to Brine-Saturated H2O
- Resistance to Chlorinated H2O
- Resistance to Clorox® (10%) H2O
- Resistance to Diesel Fuel
- Resistance to Gasoline
- Resistance to Gasoline/ 5% Methanol
- Resistance to Gasoline/5% MTBE
- Resistance to H2O
- Resistance to H2O (14 days at 82°C)
- Resistance to Hydraulic Fluid (oil)
- Resistance to Hydrochloric Acid (20%)
- Resistance to Hydrofluoric Acid(10%)
- Resistance to Isopropyl Alcohol
- Resistance to Lactic Acid
- Resistance to MEK
- Resistance to Methanol
- Resistance to Methylene Chloride
- Resistance to Mineral Spirits
- Resistance to Motor Oil
- Resistance to MTEB
- Resistance to Muriatic Acid (10%)
- Resistance to NaCl/H2O (10%)
- Resistance to Nitric Acid (20%)
- Resistance to Phosphoric Acid (10%)
- Resistance to Phosphoric Acid (50%)
- Resistance to Potassium Hydroxide (10%)
- Resistance to Potassium Hydroxide (20%)
- Resistance to Propylene Carbonate
- Resistance to Skydrol®
- Resistance to Sodium Bicarbonate
- Resistance to Sodium Hydroxide (25%)
- Resistance to Sodium Hydroxide (50%)
- Resistance to Sodium Hypochlorite (10%)
- Resistance to Steric Acid
- Resistance to Sugar/H2O
- Resistance to Sulfuric Acid (>50%)
- Resistance to Sulfuric Acid (10%)
- Resistance to Toluene
- Resistance to Trisodium Phosphate
- Resistance to Vinegar/ H2O (5%)
- Resistance to Xylene
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|