EPI Engineered Polymers EP RAP-1567 SP-HX Silicone Aliphatic Polyurea

 

Subcategory: Thermoset

Material Notes:
RAP-1567 SP is a two component 100% solids, no VOC’s, silicone aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This new generation polyurea displays fast cure times and excellent adhesion characteristics. RAP-1567 SP is designed to be quick gelling (30 minutes) in order to optimize leveling and wetting properties. RAP-1567 SP can be spray applied at temperatures ranging from 20ºF to 120ºF. This 100% polyurea elastomer displays excellent chemical resistance, water insensitivity and UV resistance (in any color) at a wide range of temperatures. RAP-1567 SP will provide a smooth glossy finish when fully cured. RAP-1567 SP emits virtually no odors and can be applied indoors without any VOC’s. RAP-1567 SP meet USDA and FDA specifications. RAP-1567 SP can be rolled, brushed, or spray applied thru airless or plural equipment.

Part of the Amber Chemical Group. Data provided by manufacturer.

Available Properties
  • Viscosity
  • Hardness, Shore D
  • Tensile Strength, Yield
  • Elongation at Yield
  • Adhesive Bond Strength
  • Tear Strength
  • Taber Abrasion, mg/1000 Cycles
  • Flash Point
  • Cure Time
  • Pot Life
  • Color
  • Flexibility
  • Resistance to 1,1,1-Trichlorethane
  • Resistance to Acetic Acid (100%)
  • Resistance to Acetone
  • Resistance to Ammonium Hydroxide (50%)
  • Resistance to Benzene
  • Resistance to Brine-Saturated H2O
  • Resistance to Chlorinated H2O
  • Resistance to Clorox® (10%) H2O
  • Resistance to Diesel Fuel
  • Resistance to Gasoline
  • Resistance to Gasoline/ 5% Methanol
  • Resistance to Gasoline/5% MTBE
  • Resistance to H2O
  • Resistance to H2O (14 days at 82°C)
  • Resistance to Hydraulic Fluid (oil)
  • Resistance to Hydrochloric Acid (20%)
  • Resistance to Hydrofluoric Acid(10%)
  • Resistance to Isopropyl Alcohol
  • Resistance to Lactic Acid
  • Resistance to MEK
  • Resistance to Methanol
  • Resistance to Methylene Chloride
  • Resistance to Mineral Spirits
  • Resistance to Motor Oil
  • Resistance to MTEB
  • Resistance to Muriatic Acid (10%)
  • Resistance to NaCl/H2O (10%)
  • Resistance to Nitric Acid (20%)
  • Resistance to Phosphoric Acid (10%)
  • Resistance to Phosphoric Acid (50%)
  • Resistance to Potassium Hydroxide (10%)
  • Resistance to Potassium Hydroxide (20%)
  • Resistance to Propylene Carbonate
  • Resistance to Skydrol®
  • Resistance to Sodium Bicarbonate
  • Resistance to Sodium Hydroxide (25%)
  • Resistance to Sodium Hydroxide (50%)
  • Resistance to Sodium Hypochlorite (10%)
  • Resistance to Steric Acid
  • Resistance to Sugar/H2O
  • Resistance to Sulfuric Acid (>50%)
  • Resistance to Sulfuric Acid (10%)
  • Resistance to Toluene
  • Resistance to Trisodium Phosphate
  • Resistance to Vinegar/ H2O (5%)
  • Resistance to Xylene
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。