EPI Engineered Polymers EP RAP-1567 SP-HX Silicone Aliphatic Polyurea
Subcategory: Thermoset
Material Notes: RAP-1567 SP-HX is a two component 100% solids, no VOC’s, silicone aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This new generation polyurea displays fast cure times and excellent adhesion characteristics. RAP-1567 SP-HX is designed to be quick gelling (30 minutes) in order to optimize leveling and wetting properties. RAP-1567 SP-HX can be spray applied at temperatures ranging from 20ºF to 120ºF. This 100% polyurea elastomer displays excellent chemical resistance, water insensitivity and UV resistance (in any color) at a wide range of temperatures. RAP-1567 SP-HX will provide a smooth glossy finish when fully cured. RAP-1567 SP-HX emits virtually no odors and can be applied indoors without any VOC’s. RAP-1567 SP-HX meet USDA and FDA specifications. RAP-1567 SP-HX can be rolled, brushed, or spray applied thru airless or plural equipment.Part of the Amber Chemical Group. Data provided by manufacturer.
| Available Properties |
- Viscosity
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Yield
- Adhesive Bond Strength
- Tear Strength
- Taber Abrasion, mg/1000 Cycles
- Flash Point
- Cure Time
- Pot Life
- Color
- Flexibility
- Resistance to 1,1,1-Trichlorethane
- Resistance to Acetic Acid (100%)
- Resistance to Acetone
- Resistance to Ammonium Hydroxide (50%)
- Resistance to Benzene
- Resistance to Brine-Saturated H2O
- Resistance to Chlorinated H2O
- Resistance to Clorox® (10%) H2O
- Resistance to Diesel Fuel
- Resistance to Gasoline
- Resistance to Gasoline/ 5% Methanol
- Resistance to Gasoline/5% MTBE
- Resistance to H2O
- Resistance to H2O (14 days at 82°C)
- Resistance to Hydraulic Fluid (oil)
- Resistance to Hydrochloric Acid (20%)
- Resistance to Hydrofluoric Acid(10%)
- Resistance to Isopropyl Alcohol
- Resistance to Lactic Acid
- Resistance to MEK
- Resistance to Methanol
- Resistance to Methylene Chloride
- Resistance to Mineral Spirits
- Resistance to Motor Oil
- Resistance to MTEB
- Resistance to Muriatic Acid (10%)
- Resistance to NaCl/H2O (10%)
- Resistance to Nitric Acid (20%)
- Resistance to Phosphoric Acid (10%)
- Resistance to Phosphoric Acid (50%)
- Resistance to Potassium Hydroxide (10%)
- Resistance to Potassium Hydroxide (20%)
- Resistance to Propylene Carbonate
- Resistance to Skydrol®
- Resistance to Sodium Bicarbonate
- Resistance to Sodium Hydroxide (25%)
- Resistance to Sodium Hydroxide (50%)
- Resistance to Sodium Hypochlorite (10%)
- Resistance to Steric Acid
- Resistance to Sugar/H2O
- Resistance to Sulfuric Acid (>50%)
- Resistance to Sulfuric Acid (10%)
- Resistance to Toluene
- Resistance to Trisodium Phosphate
- Resistance to Vinegar/ H2O (5%)
- Resistance to Xylene
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|