Sun Plastech ASACLEAN Purging Compound Type UP Grade
Subcategory: Purging Compound; Thermoplastic; Olefinic TPE
Key Words: ASACLEAN, Asahi Kasei, Purge
Material Notes: Specifically for Polypropylene, Purging compound for plastic injection molding machines and extrudersProcessing Notes: Purging to and from polypropylene based resins within temperature range Information provided by Asaclean - Sun Plastech Inc.
|
|
|