Advanced Elastomer Systems Santoprene® 171-64 Thermoplastic Rubber
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: A black thermoplastic specialty elastomer which complies with FDA regulations for rubber articles intended for repeated use, as well as rubber articles in contact with non-fatty, non-oily foods as closures and sealing gaskets, formulated to replace thermoset elastomers like EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be processed using injection molding, extrusion, blow molding or other melt processing techniques. Key Features: Dielectric constant 2.3, dielectric strength at 3.17 mm (125 mil), 19.6 kV/mm (500 v/mil); UL Yellow Card listed, UL 94 HB flame rating; Continuous temperature rating 1000 hrs. @ 135°C (275°F); Excellent flex fatigue resistance; Complies with 21 CFR 177.1210 "Closures with Sealing Gaskets for Food Containers"; Complies with 21 CFR 177.2600 "Rubber Articles Intended for Repeated Use" Additional processing comments: This thermoplastic rubber is a shear-dependent material that can be processed on conventional thermoplastic equipment for injection molding, extrusion, or blow molding. For extrusion, a general purpose screw with a compression ratio of 2.5 to 3.0 is recommended. Material can be recycled. SANTOPRENE rubber is incompatible with acetal and PVC. Values below are for injection molded plaques, side gated, 82.6 mm x 117.5 mm x 3.0 mm. Tensile properties measured across flow. Data provided by Advanced Elastomer Systems.
| Available Properties |
- Density
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 100% Modulus
- Graves Tear Strength
- Compression Set
- Compression Set, Elevated Temperature
- Tensile Set
- Dielectric Constant
- Dielectric Strength
- Maximum Service Temperature, Air
- Brittleness Temperature
- Flammability, UL94
- Processing Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|