Advanced Elastomer Systems Santoprene™ TPV 8201-80 Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Thermoplastic; Thermoplastic Vulcanizate Elastomer (TPV)
Key Words: EU 2003/11/EC; RoHS Compliant; UL JMLU2; UL QMFZ2; UL QMFZ8
Material Notes: A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range of applications. This grade of Santoprene 8000 TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable.- Non-hygroscopic product, requires little to no drying before processing.
- Neutral, easy coloring formulation.
- Recommended for applications requiring excellent ozone resistance.
- Used in sealing applications.
- Recommended for applications requiring excellent flex fatigue resistance.
- Blow Molding Applications
- Industrial Applications
- Profiles
- Sporting Goods
- Telecommunications
- Tubing
- Wheels
Information provided by Advanced Elastomer Systems
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Tensile Strength @ Break
- Elongation at Break
- Tear Strength
- Compression Set
- Volume Resistivity
- Brittleness Temperature
- Processing Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Die Temperature
- Melt Temperature
- Mold Temperature
- Moisture Content
- Back Pressure
- Clamp Pressure
- Vent Depth
- Cushion
- Screw Speed
- Color
- Form
- Injection Rate
- Maximum Regrind %
- Screw Compression Ratio
- Screw L/D Ratio
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|