Advanced Elastomer Systems Santoprene™ TPV 8211-55 Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Thermoplastic; Thermoplastic Vulcanizate Elastomer (TPV)
Key Words: EU 2003/11/EC; RoHS Compliant; UL QMFZ2; UL QMFZ8
Material Notes: A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult injection molding applications. This grade of Santoprene 8000 TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding. It is polyolefin based and completely recyclable.- Non-hygroscopic product, requires little to no drying before processing.
- Neutral, easy coloring formulation.
- Recommended for applications requiring excellent ozone resistance.
- Used in sealing applications.
- Recommended for applications requiring excellent flex fatigue resistance.
- Consumer Applications
- Grips, Flexible
- Hinges, Living
- Industrial Applications
- Low Temperature Applications
- Parts, Thin-walled
- Toys
- Writing Instruments
Information provided by Advanced Elastomer Systems
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Tensile Strength @ Break
- Elongation at Break
- Compression Set
- Brittleness Temperature
- Processing Temperature
- Mold Temperature
- Moisture Content
- Back Pressure
- Clamp Pressure
- Vent Depth
- Cushion
- Screw Speed
- Color
- Form
- Injection Rate
- Maximum Regrind %
- Screw Compression Ratio
- Screw L/D Ratio
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|