Advanced Elastomer Systems Santoprene™ TPV 121-50E500 Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Thermoplastic; Thermoplastic Vulcanizate Elastomer (TPV)
Key Words: EU 2003/11/EC; RoHS Compliant
Material Notes: A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has controlled rheology for robotic or specialty extrusion applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for extrusion. It is polyolefin based and completely recyclable.- Designed for applications requiring good elastic recovery.
- Designed for improved UV resistance.
- Recommended for applications requiring superior part surface appearance.
Information provided by Advanced Elastomer Systems
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Tensile Strength @ Break
- Elongation at Break
- Compression Set
- Brittleness Temperature
- Processing Temperature
- Color
- Form
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|