Advanced Elastomer Systems Santoprene™ TPV 121-65M300 Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Thermoplastic; Thermoplastic Vulcanizate Elastomer (TPV)
Key Words: EU 2003/11/EC; RoHS Compliant
Material Notes: A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and good appearance. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding. It is polyolefin based and completely recyclable.- Designed for fast, easy injection molding, especially for complex part geometries.
- Used in sealing applications.
- Recommended for applications requiring superior part surface appearance.
- Designed to be injected at lower molding temperatures or at lower injection pressures.
- Designed for automotive interior applications requiring low fogging and low odor.
Information provided by Advanced Elastomer Systems
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Tensile Strength @ Break
- Elongation at Break
- Compression Set
- Brittleness Temperature
- Processing Temperature
- Color
- Form
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|