Advanced Elastomer Systems Santoprene™ TPV 121-79W233 Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Thermoplastic; Thermoplastic Vulcanizate Elastomer (TPV)
Key Words: EU 2003/11/EC; RoHS Compliant
Material Notes: A soft, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated to bond to sulfur or peroxide-cured thermoset EPDM rubber for corner molding, end caps and special fixation applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding. It is polyolefin based and completely recyclable.- Designed for applications requiring excellent adhesion to vulcanized EPDM rubber.
- Specially formulated to replace thermoset EPDM rubber in automotive glass run channel corner molding applications.
- Designed for shorter processing time compared to thermoset EPDM rubber.
Information provided by Advanced Elastomer Systems
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Tensile Strength @ Break
- Elongation at Break
- Tear Strength
- Compression Set
- Brittleness Temperature
- Processing Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Back Pressure
- Clamp Pressure
- Vent Depth
- Cushion
- Screw Speed
- Color
- Form
- Injection Rate
- Maximum Regrind %
- Screw Compression Ratio
- Screw L/D Ratio
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|