Advanced Elastomer Systems Santoprene™ TPV 171-64 Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Thermoplastic; Thermoplastic Vulcanizate Elastomer (TPV)
Key Words: EU 2003/11/EC; FDA 21 CFR 177.1210; FDA 21 CFR 177.2600; NSF 51; RoHS Compliant; UL QMFZ2; UL QMFZ8
Material Notes: A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those in contact with non-fatty, non-oily foods as closures and sealing gaskets. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable.Recommended for applications requiring excellent flex fatigue resistance. Information provided by Advanced Elastomer Systems
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Tensile Strength @ Break
- Elongation at Break
- Tear Strength
- Compression Set
- Brittleness Temperature
- Processing Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Die Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Back Pressure
- Clamp Pressure
- Vent Depth
- Cushion
- Screw Speed
- Color
- Form
- Injection Rate
- Maximum Regrind %
- Screw Compression Ratio
- Screw L/D Ratio
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|