Advanced Elastomer Systems Santoprene™ TPV 241-87 Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Thermoplastic; Thermoplastic Vulcanizate Elastomer (TPV)
Key Words: EU 2003/11/EC; NSF 61; RoHS Compliant
Material Notes: A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 for food processing equipment. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable.- Complies with NSF Standard 51: Listed Plastic Materials and Components used in Food Equipment.
- Complies with NSF Standard 61: Piping System Components for Drinking Water.
- Recommended for applications requiring excellent flex fatigue resistance.
Information provided by Advanced Elastomer Systems
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Tensile Strength @ Break
- Elongation at Break
- Compression Set
- Processing Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Die Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Back Pressure
- Clamp Pressure
- Vent Depth
- Cushion
- Screw Speed
- Change in Mass in IRM 903 Oil at 257°F for 70 hr
- Color
- Form
- Injection Rate
- Maximum Regrind %
- Screw Compression Ratio
- Screw L/D Ratio
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|