Advanced Elastomer Systems Santoprene™ TPE 912BA Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Thermoplastic; Thermoplastic Vulcanizate Elastomer (TPV)
Key Words: EU 2003/11/EC; RoHS Compliant
Material Notes: A hard, black, super high-flow thermoplastic olefin (TPO) in the thermoplastic elastomer (TPE) family. This grade of Vistaflex TPE is temperature-dependent and can be processed on conventional thermoplastics equipment for injection molding. It is polyolefin based and completely recyclable.Recommended for applications requiring good UV resistance, impact resistance, paintability, high flow and medium modulus. Recommended for applications requiring superior part surface appearance. Information provided by Advanced Elastomer Systems
| Available Properties |
- Melt Flow
- Change in Mass in IRM 903 Oil at 257°F for 70 hr
- Color
- Form
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|