Advanced Elastomer Systems Santoprene® 151-60 Thermoplastic Rubber
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: Description: A black thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be processed using injection molding, extrusion, blow molding or other melt processing techniques. Supplied as free-flowing pellets in 25 kilogram (55 pound) moisture barrier bags. Features: - Excellent flex fatigue resistance
- Excellent Ozone Resistance
Product Notes: Values are for injection molded plaques, side gated. 102 mm x 152 mm x 2 mm Information provided by Advanced Elastomer Systems.
| Available Properties |
- Density
- Hardness, Shore A
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Flammability, UL94
- Oxygen Index
- Processing Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|