Advanced Elastomer Systems Santoprene® 221-80 Thermoplastic Rubber
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: Description: A colorable thermoplastic specialty elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be processed using injection molding, extrusion, blow molding or other melt processing techniques. Supplied as free-flowing pellets in 25 kilogram (55 pound) moisture barrier bags. Features: - Excellent flex fatigue resistance
- Excellent ozone resistance
- Excellent mechanical properties retention after UV exposure
- Minimal part warpage
- Can be injected at lower molding temperatures or at lower injection pressures
- Low odor
- Very low fogging
Product Notes: Values are for injection molded plaques, side gated. 82.6 mm x 117.5 mm x 3 mm Information provided by Advanced Elastomer Systems.
| Available Properties |
- Density
- Hardness, Shore A
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Maximum Service Temperature, Air
- Brittleness Temperature
- Processing Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|