Advanced Elastomer Systems Santoprene® 241-73W236 Thermoplastic Rubber
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: Description: A colorable thermoplastic specialty elastomer designed for use in food processing equipment and plumbing applications in contact with potable water. It contains a stabilization system for protection against copper and other metal-catalyzed degradation, and can be processed using injection molding, extrusion, blow molding or other melt processing techniques. Supplied as free-flowing pellets in 25 kilogram (55 pound) moisture barrier bags. Features: - Expected to comply with NSF Standard 51: Listed plastic materials and components used in food equipment
- Expected to comply with NSF Standard 61: Piping system components for drinking water
Product Notes: Values are for injection molded plaques, side gated. 82.6 mm x 117.5 mm x 3 mm Information provided by Advanced Elastomer Systems.
| Available Properties |
- Density
- Hardness, Shore A
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Tear Strength
- Compression Set
- Tensile Set
- Brittleness Temperature
- Processing Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|