Advanced Elastomer Systems Santoprene® 8271-80HT Thermoplastic Rubber
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: Description: A colorable thermoplastic elastomer which complies with FDA regulations for rubber articles intended for repeated use. It can be processed using injection molding or extrusion melt processing techniques. The material offers enhanced tensile, tear, and abrasion properties along with improved processability and finished part appearance. Supplied as free-flowing pellets in 25 kilogram (55 pound) moisture barrier bags. Product Notes: Values are for injection molded plaques, side gated. 82.6 mm x 117.5 mm x 3 mm Information provided by Advanced Elastomer Systems.
| Available Properties |
- Density
- Hardness, Shore A
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Tear Strength
- Abrasion
- Compression Set
- Tensile Set
- Flammability, UL94
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|