Advanced Elastomer Systems VistaFlex® 715-N Thermoplastic Rubber
Subcategory: Elastomer, TPE; Thermoplastic
Close Analogs: This grade is no longer a commercial product
Material Notes: Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-flowing pellets in 25 kilogram (55 pound) moisture barrier bags. Features: - High flow
- Good surface appearance on molded parts
- Good tensile properties
- Good tear strength
Product Notes: Values are for injection molded plaques, side gated. 82.6 mm x 117.5 mm x 3 mm Information provided by Advanced Elastomer Systems.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore A
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Tear Strength
- Compression Set
- Izod Impact, Notched @ -30°C
- Vicat Softening Point
- Brittleness Temperature
- Processing Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|