Asahi Glass Co. Lumiflon® LF-810 Solvent Soluble Fluoropolymer
Subcategory: Fluoropolymer; Thermoplastic
Material Notes: Lumiflon was developed by Asahi Glass in 1982, and is unique being the first solvent soluble fluoropolymer. The FEVE based Lumiflon has a alternative copolymer. The complete inter-changeability between the Fluoroethylene and Alkyl Vinyl Ether gives excellent weathering and a high chemical resistance. LF-810 is designed for use with mineral spirits for use in repair coatings and aged surfaces.Information provided by Asahi Glass Company, Inc.
| Available Properties |
- Specific Gravity
- Solids Content
- Viscosity Measure
- Molecular Weight
- Acid Value
- Glass Temperature
- Appearance
- OH Value mgKOH/g
- Solvent
|
|
|
|
| Property Data |