Asahi Glass Co. Lumiflon® LF-200 Solvent Soluble Fluoropolymer w/ isocyanate hardening agent

 

Subcategory: Fluoropolymer; Thermoplastic

Material Notes:
Lumiflon was developed by Asahi Glass in 1982, and is unique being the first solvent soluble fluoropolymer. The FEVE based Lumiflon has a alternative copolymer. The complete inter-changeability between the Fluoroethylene and Alkyl Vinyl Ether gives excellent weathering and a high chemical resistance. LF-200 is the general purpose product. The coating is used both in air dry systems and also in baking. It is being used to form the backbone of coatings for off shore oil platforms and as clear coat for plastic parts on cars and major appliances. LF-200 can be found in heavy duty applications such as bridges, plants and architectural exteriors.

Information provided by Asahi Glass Company, Inc.

Available Properties
  • Specific Gravity
  • Solids Content
  • Viscosity Measure
  • Acid Value
  • Impact
  • Glass Temperature
  • Gloss
  • Appearance
  • Erichsen Test
  • OH Value mgKOH/g
  • Pencil Hardness
  • Solubility Parameter
  • Solvent
  • T-bend test (no cracking)
  • Xylol Rubbing Test
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。