Asahi Glass Co. AFLAS® MZ TFE/P/VdF Fluoroelastomer
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset; PVDF
Material Notes: AFLAS® MZ is a terpolymer composed of tetrafluoroethylene, propylene and vinylidene fluoride. AFLAS® MZ offers a good balance of chemical resistance and improved low temperature performance and is categorized in ASTM D 1418-01 as class FKM, type four.Information provided by Asahi Glass Company, Inc.
| Available Properties |
- Specific Gravity
- Mooney Viscosity
- Hardness, Shore A
- Tensile Strength at Break
- Elongation at Break
- Compression Set, Elevated Temperature
- Glass Temperature
- Flourine Content %
|
|
|
|