Asahi Glass Co. Fluon® PA1020Z 20% Glass Fiber, PTFE Filled Compound
Subcategory: Fluoropolymer; Thermoplastic; PTFE; Polymer
Material Notes: Fluon®PTFE FC has improved creep and wear resistance. A wide range of fillers such as glass fiber, graphite, bronze, carbon fiber are available. Information provided by Asahi Glass Company, Inc.
| Available Properties |
- Specific Gravity
- Bulk Density
- Particle Size
- Tensile Strength at Break
- Elongation at Break
- PTFE Content, %
|
|
|
|