Asahi Glass Co. Fluon® P-62XP PFA Perfluoropolymer
Subcategory: Fluoropolymer; Thermoplastic; PFA
Material Notes: Fluon®PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent characteristics and similar properties of PTFE but can be processed using conventional thermoplastic techniques, such as extrusion molding, injection molding, blow molding, or electrostatic powder coating. And Fluon®PFA can be used in a wide range of temperatures from extremely low to high temperatures (260°C at the maximum) without losing its superior properties. Information provided by Asahi Glass Company, Inc.
| Available Properties |
- Specific Gravity
- Water Absorption
- Melt Flow
- Hardness, Shore D
- Tensile Strength at Break
- Tensile Strength, Ultimate at Elevated Temperature
- Elongation at Break
- Elongation at Break at Elevated Temperature
- Flexural Modulus
- Coefficient of Friction
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dissipation Factor
- Arc Resistance
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Flammability, UL94
- Oxygen Index
- Flex Life, Cycles
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|