Asahi Glass Co. Fluon® P-830UP PFA Perfluoropolymer

 

Subcategory: Fluoropolymer; Thermoplastic; PFA

Material Notes:
Fluon®PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent characteristics and similar properties of PTFE but can be processed using conventional thermoplastic techniques, such as extrusion molding, injection molding, blow molding, or electrostatic powder coating. And Fluon®PFA can be used in a wide range of temperatures from extremely low to high temperatures (260°C at the maximum) without losing its superior properties.

Information provided by Asahi Glass Company, Inc.

Available Properties
  • Specific Gravity
  • Water Absorption
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength at Break
  • Tensile Strength, Ultimate at Elevated Temperature
  • Elongation at Break
  • Elongation at Break at Elevated Temperature
  • Flexural Modulus
  • Coefficient of Friction
  • Izod Impact, Notched
  • Volume Resistivity
  • Surface Resistance
  • Dielectric Constant
  • Dissipation Factor
  • Arc Resistance
  • CTE, linear 20°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Maximum Service Temperature, Air
  • Flammability, UL94
  • Oxygen Index
  • Flex Life, Cycles
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。