Akzo Nobel Trigonox® C Polymerization Initiator
Subcategory: Polymer
Material Notes: Initiator for the (co)polymerization of ethylene, styrene, acrylonitrile, vinylacetate, acrylates and methacrylates. Trigonox C is a monofunctional peroxide which is used for the crosslinking of polyolefins as well as natural rubber and synthetic rubbers. Trigonox C may also be used for the curing of unsaturarated polyester, vinylester and thermoset acrylic resins at elevated temperatures Chemical Description: tert-Butyl peroxybenzoate CAS Number: 614-45-9 Acronym: TBPB; Tx C Information provided by Akzo Nobel Polymer Chemicals.
| Available Properties |
- One Hour Half Life Temperature
- Storage Temperature
|
|
|
|
| Property Data |