Akzo Nobel Trigonox® C-50D-pd Peroxide Cure Agent
Subcategory: Polymer
Material Notes: Trigonox C-50D-pd is a monofunctional peroxide which is used for the crosslinking of polyolefins as well as natural rubber and synthetic rubbers. Chemical Description: tert-Butyl peroxybenzoate, powder, 50% with inert fillers CAS Number: 614-45-9 Acronym: TBPB; Tx C Information provided by Akzo Nobel Polymer Chemicals.
| Available Properties |
- One Hour Half Life Temperature
- Storage Temperature
|
|
|
|