Akzo Nobel Trigonox® D-C50 Polymerization Initiator
Subcategory: Polymer
Material Notes: Initiator for the (co)polymerization of ethylene, styrene, acrylonitrile, acrylates and methacrylates. Trigonox D-C50 may also be used as an initiator for curing unsaturated polyester and vinylester resins at elevated temperatures. Chemical Description: 2,2-Di(tert-butylperoxy)butane, 50% solution in odorless mineral spirits CAS Number: 2167-23-9 Acronym: Tx D Information provided by Akzo Nobel Polymer Chemicals.
| Available Properties |
- One Hour Half Life Temperature
- Storage Temperature
|
|
|
|