Akzo Nobel Trigonox® EHP-C65 Polymerization Initiator
Subcategory: Polymer
Material Notes: Initiator for the (co)polymerization of ethylene, vinylchloride, vinylidenechloride, acrylates and methacrylates. Chemical Description: Di(2-ethylhexyl) peroxydicarbonate, 65% solution in odorless mineral spirits CAS Number: 16111-62-9 Acronym: EHP; OPP; Tx EHP Information provided by Akzo Nobel Polymer Chemicals.
| Available Properties |
- One Hour Half Life Temperature
- Storage Temperature
|
|
|
|