Akzo Nobel Trigonox® HM Peroxide Cure Agent
Subcategory: Polymer
Material Notes: Trigonox HM is a peroxide formulation for the curing of unsaturated polyester resins as such or in the presence of a cobalt accelerator. Chemical Description: Methyl isobutyl ketone peroxide, 45% solution in diisobutyl phthalate CAS Number: 37206-20-5; 12262-58-7 Acronym: MIBKP; Tx HM Information provided by Akzo Nobel Polymer Chemicals.
|
|
|