Akzo Nobel Trigonox® TAHP-W85 Polymerization Initiator
Subcategory: Polymer
Material Notes: Initiator for the (co)polymerization of styrene, acrylonitrile, acrylates and methacrylates. Chemical Description: tert-Amylhydroperoxide, 85% solution in water CAS Number: 3425-61-4 Acronym: TAHP; Tx TAHP Information provided by Akzo Nobel Polymer Chemicals.
| Available Properties |
- One Hour Half Life Temperature
- Storage Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|