Honeywell Aegis™ OX High Barrier Nylon

 

Subcategory: Nylon; Thermoplastic; Polymer

Material Notes:
Description: Aegis OX is an oxygen-scavenging nylon. Oxygen barrier is comparable to a glass bottle with metal crown closure. In addition Aegis OX provides CO2 barrier and possesses glass-like clarity. Because the recommended processing temperature of Aegis OX is similar to PET's, Aegis OX is well suited to the PET co-injection process and provides excellent adhesion to PET. Aegis OX is also delamination resistant and recyclable.

Information provided by Honeywell.

Available Properties
  • Specific Gravity
  • Oxygen Transmission
  • Carbon Dioxide Transmission
  • Melt Index of Compound
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Yield
  • Secant Modulus
  • Transformation Temperature, Tg
  • Processing Temperature
  • Feed Temperature
  • Nozzle Temperature
  • Zone 1
  • Zone 2
  • Zone 3
  • Zone 4
  • Zone 5
  • Melt Temperature
  • Oxygen Scav. Capacity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。