Honeywell Aegis™ OX High Barrier Nylon
Subcategory: Nylon; Thermoplastic; Polymer
Material Notes: Description: Aegis OX is an oxygen-scavenging nylon. Oxygen barrier is comparable to a glass bottle with metal crown closure. In addition Aegis OX provides CO2 barrier and possesses glass-like clarity. Because the recommended processing temperature of Aegis OX is similar to PET's, Aegis OX is well suited to the PET co-injection process and provides excellent adhesion to PET. Aegis OX is also delamination resistant and recyclable.Information provided by Honeywell.
| Available Properties |
- Specific Gravity
- Oxygen Transmission
- Carbon Dioxide Transmission
- Melt Index of Compound
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Secant Modulus
- Transformation Temperature, Tg
- Processing Temperature
- Feed Temperature
- Nozzle Temperature
- Zone 1
- Zone 2
- Zone 3
- Zone 4
- Zone 5
- Melt Temperature
- Oxygen Scav. Capacity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|