Honeywell ACLAM® TC200 (10.0 mil), Low Temperature, Heat Sealable Lamination
Subcategory: Thermoplastic; Polymer
Material Notes: Description: ACLAR® TC200 is a low temperature heat sealable lamination composed of a 2 mil polyolefin heat seal layer and a 8 mil proprietary Aclar® 11C film layer.Information provided by Honeywell.