Honeywell ACLAR® 22A (1.50 mil), Copolymer Film
Subcategory: Fluoropolymer; Thermoplastic; Polymer
Material Notes: Description: ACLAR® 22A is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It is a flexible transparent film used to package moisture sensitive products.Information provided by Honeywell.
| Available Properties |
- Specific Gravity
- Density
- Water Vapor Transmission
- Thickness
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Tear Strength Test
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Thermal Conductivity
- Melting Point
- Oxygen Index
- Shrinkage, MD
- Shrinkage, TD
- Haze
- Flammability
|
|
|
|