BASF Petra 140 PET, 45% Glass Filled
Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic
Material Notes: Information provided by BASF Corporation.
| Available Properties |
- Density
- Melt Density
- Viscosity Measurement
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Unnotched
- Charpy Impact, Notched
- Izod Impact, Notched
- Volume Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Melt Temperature
- Mold Temperature
- Fill Speed
- Additive
- Color
- Commercial Status (March 2007)
- Form
- Impact Modified
- Injection molding
- Primary Processing Technique
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|