BASF Ultradur S 4090 G6 PBT, 30% Glass Filled
Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic
Material Notes: Information provided by BASF Corporation.
| Available Properties |
- Density
- Melt Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Viscosity Test
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Charpy Impact Unnotched
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Tensile Creep Modulus, 1 hour
- Tensile Creep Modulus, 1000 hours
- Izod Impact, Notched @ -40°C
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dissipation Factor
- Comparative Tracking Index
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Melt Temperature
- Mold Temperature
- Fill Speed
- Additive
- Attribute
- Color
- Commercial Status (March 2007)
- Form
- Impact Modified
- Injection molding
- Primary Processing Technique
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|