BASF Ultramid B3 Nylon 6 (Conditioned) (America and Europe)
Subcategory: Nylon; Thermoplastic; Nylon 6
Close Analogs: This product is not listed in the BASF product line, March 2007.
Material Notes: Not Impact modified. Information provided by BASF.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact, Notched
- Tensile Creep Modulus, 1000 hours
- Melting Point
- Color
- Primary Processing
|
|
|
|
| Property Data |