Honeywell Capran® Emblem™ 1200Matte, Matte Coated Bi-Axially Oriented Nylon Film
Subcategory: Nylon; Thermoplastic; Polymer
Material Notes: Description: Capran® Emblem™ 1200Matte is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbons, and many solvents. It is also microwavable, making it an excellent choice for lidding stock. 1200Matte film has a matte appearance on one side. The matte surface provides superior scuff resistance while maintaining excellent contact clarity. Applications: thermal lamination films used in book cover applications. Information provided by Honeywell.
| Available Properties |
- Density
- Thickness
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Coefficient of Friction
- Tear Strength Test
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Shrinkage, MD
- Shrinkage, TD
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|