Honeywell Capran® Emblem™ 1200MT, Bi-Axially Oriented Nylon Film
Subcategory: Nylon; Thermoplastic; Polymer
Material Notes: Description: Capran® Emblem™ 1200MT is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbons, and many solvents. It is also microwavable, making it an excellent choice for lidding stock. 1200MT film has a metallized coating that provides an effective barrier to oxygen, helium, and water vapor. Applications: message balloons as well as food packaging requiring high barrier. Information provided by Honeywell.
| Available Properties |
- Density
- Water Vapor Transmission
- Oxygen Transmission Rate
- Thickness
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Coefficient of Friction
- Tear Strength Test
- Elmendorf Tear Strength, MD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Shrinkage, MD
- Shrinkage, TD
- Helium Transition Rate
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|