Honeywell Capran® Emblem™ MT2500, Bi-Axially Oriented Nylon 6 Film
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Material Notes: Description: Capran® Emblem™ MT2500 is a 1.00 mil (25 micron) biaxially oriented nylon 6 film with a metallized barrier coating.Applications: Capron® Emblem™ MT2500 is well suited for high barrier packaging solutions. Information provided by Honeywell.
| Available Properties |
- Density
- Water Vapor Transmission
- Oxygen Transmission Rate
- Thickness
- Surface Tension
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Coefficient of Friction
- Tear Strength Test
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Shrinkage, MD
- Shrinkage, TD
- Helium Transition Rate
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|